III-V Etcher and Atomic Layer Etching (ALE): Oxford Instruments PlasmaPro 100 Cobra 300 ICP-RIE with ALE

From the KNI Lab at Caltech
Revision as of 00:21, 1 October 2026 by Kmmckenz (talk | contribs) (Created page with "{{InstrumentInfoboxOneImage| |InstrumentName = III-V, Metal & Si Etcher |HeaderColor = #FFE2B9 |ImageOne = ICP-RIE_III-V,Metal,Si-Etcher.jpg |ImageTwo = |InstrumentType = Etching |RoomLocation = B235 Steele |LabPhone = 626-395-1532 |PrimaryStaff = Kelly McKenzie |StaffEmail = kmmckenz@caltech.edu |StaffPhone = 626-395-5732 |Manufacturer = Oxford Instruments |Techniques = pseudo-Bosch & Cryogenic Si Etch<br>Compound Semiconductor Etching |E...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search
III-V, Metal & Si Etcher
Instrument Type Etching
Techniques pseudo-Bosch & Cryogenic Si Etch
Compound Semiconductor Etching
Staff Manager Kelly McKenzie
Staff Email kmmckenz@caltech.edu
Staff Phone 626-395-5732
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B235 Steele
Lab Phone 626-395-1532
Manufacturer Oxford Instruments
Model Plasmalab System 100

Description

The III-V, Metal & Silicon inductively-coupled plasma reactive-ion etcher (ICP-RIE) is an Oxford Instruments Plasma Technology Plasmalab System 100 ICP-RIE 380 system that is optimized for the etching of compound semiconductors, metals, and silicon. In addition to a wide range of gases for etching a variety of III-V materials and metals, this system is configured for highly-selective ICP-RIE of silicon via the pseudo-Bosch process, allowing silicon etching with SF6 and C4F8 gases as well as cryogenic silicon etching with SF6 and O2 over a temperature range of -140 to 300 °C. This system supports wafer sizes up to 6 inches.

Applications
  • InP grating etch
  • GaAs photonics device etch
  • pseudo-Bosch of silicon
  • Metals etch
  • Cryogenic etch of silicon (available upon request)
Allowed Material in Etcher
  • Etch materials: Si, SixNy, SiO2, Ge, InP, GaAs, Al, Mo, Nb, W, Ti
  • Masks: PMMA/ZEP/SPR/AZ/maN resists, SiOx/Al2O3, Cr hard masks
  • Other: Metal in etch stack (not exposed to plasma)
Etching Gas List
  • SF6
  • C4F8
  • O2
  • Ar
  • Cl2
  • SiCl4
  • CH4
  • H2
  • HBr

Resources

SOPs & Troubleshooting
Process Documents
Review Articles
Manufacturer Manuals

Specifications

Manufacturer Specifications
System Features
  • Universal base console that houses the electronic sub systems, control units, pneumatics, and turbomolecular pump
  • PC 2000 Operating system
  • ICP process chamber with 200 mm pumping port, view port and end-point-detection ports for optical emission spectrometer and laser interferometer
  • Variable height 240 mm Cryo RIE electrode
  • Parameter ramping software (Not Bosch)
  • 100-mTorr, temperature-stabilized capacitance manometer for process control with an active penning gauge for base pressure measurement
  • 200 mm pumping port is fitted with a 200 mm variable gate valve for chamber isolation and process pressure control
  • Twelve line gas pod with three non-toxic and six toxic digital mass-flow-controlled gas lines
  • Alcatel 1300 l/s MAGLEV turbo pump
  • Single-wafer automatic insertion load lock with soft pump option
System Specifications
  • Chamber wall heating 80 °C
  • Cryo table range -140 to 400 °C
  • ICP 380 mm remote high-density plasma source with 5 kW RF generator and automatic matching unit close-coupled to the source
  • Substrate bias control by 30 / 300 W RIE source