Contact Mask Aligners: MA6 & MA6/BA6: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
Derose (talk | contribs)
No edit summary
Bertm (talk | contribs)
Line 32: Line 32:
* [https://caltech.box.com/s/j19tuhv68bk0nsa5nruc95g4dizzxtr7 Lithography Pass-down equipment information]
* [https://caltech.box.com/s/j19tuhv68bk0nsa5nruc95g4dizzxtr7 Lithography Pass-down equipment information]
===== SOPs & Troubleshooting =====
===== SOPs & Troubleshooting =====
*Tool Reservation Rules
{| class="wikitable"
|-
!  !! Advanced Reservation (days) !! Limit per Reservation (hrs) !! Limit per week (hrs)
|-
| Weekday || 7 || 4 || 12
|-
| Weeknight || 7 || 4 || 16
|-
| Weekend || 14 || 4 || 16
|}
* [https://caltech.box.com/s/gkhncvqe25uccym7cs5aj0n00krbmnw1 General SOP & Troubleshooting]
* [https://caltech.box.com/s/gkhncvqe25uccym7cs5aj0n00krbmnw1 General SOP & Troubleshooting]
* [https://caltech.box.com/s/bbk4f9vi6jerhi9fcqoqa78n5npkwxkr Lamp Change SOP]
* [https://caltech.box.com/s/bbk4f9vi6jerhi9fcqoqa78n5npkwxkr Lamp Change SOP]

Revision as of 01:02, 27 May 2022

Suss Contact Mask Aligner MA6/BA6
Instrument Type Lithography
Techniques Frontside Alignment,
Backside Alignment,
Flood exposure
Staff Manager Alireza Ghaffari
Staff Email ghaffari@caltech.edu
Staff Phone 626-395-3984
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B217 Steele
Lab Phone 626-395-1535
Manufacturer Suss MicroTec
Model MA6 & MA6/BA6

Description

Suss MicroTec model MA6 Mask Aligner (model MA6/BA6 is shown at the top of the infobox)

The contact mask aligner is a tool that enables front- and back-side alignment of photo masks to create structures as small as 500 nm on sample sizes up to 6 inches. These systems are ideally suited for rapid definition of sub-micron devices through contact printing, and enable the high-resolution alignment of several lithographic layers to define complex devices. They are typically used to define contacts and connections to the nanostructures that are defined using the KNI's other fabrication instruments (e.g. e-beam lithography). The MA6/BA6 is also configured to do bond aligning in support of the Suss Microtec SB6L Wafer Bonder.

Suss1 MA6/BA6 Applications
  • Front Side Flood Exposure (no mask)
  • Front Side Alignment & Exposure
  • Back Side Alignment with Front Side Exposure
Suss2 MA6 Applications
  • Front Side Alignment & Exposure
  • Back Side Alignment with Front Side Exposure

Resources

Equipment Data
SOPs & Troubleshooting
  • Tool Reservation Rules
Advanced Reservation (days) Limit per Reservation (hrs) Limit per week (hrs)
Weekday 7 4 12
Weeknight 7 4 16
Weekend 14 4 16
Optical Lithography Resources
Process Recipes
Manufacturer Manuals

Specifications

Manufacturer Specifications
  • Whole wafers 2” up to 6” can be loaded.
  • Samples pieces up to 6”x6” square can be loaded.
  • Samples up to 6mm thick can be loaded..
  • Exposure Resolution:
Soft Contact Mode = 1 - 2 um
Hard Contact Mode = 1 um
Soft Vacuum Contact Mode = 1 - 0.5 um
Vacuum Contact Mode = 0.4 - 0.5 um
Suss 1 Exposure Settings
  • Channel 1 is 365nm wavelength at 15 mW/cm2.
  • Channel 2 is 405nm wavelength at 25 mW/cm2.
Suss 2 Exposure Settings
  • Channel 1 is 365nm wavelength at 10 mW/cm2.
  • Channel 2 is 405nm wavelength at 15 mW/cm2.
Electron Beam Lithography
Ion Beam Lithography
Optical Lithography