Labline: Electron Beam Evaporator: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
Derose (talk | contribs)
Sydney (talk | contribs)
m Removed link to Equipment Status under Resources since the status can be viewed directly by users in FBS, per Tiffany 4/15/24 sg
(3 intermediate revisions by 2 users not shown)
Line 26: Line 26:


== Resources ==
== Resources ==
===== Equipment Data =====
* [https://caltech.box.com/s/lul90odaqj4rp9inb6qt2mft2ean0qqa Deposition Pass-down equipment information]
===== SOPs & Troubleshooting =====
===== SOPs & Troubleshooting =====
* [https://caltech.box.com/s/9sx2vhd9gz5rdhviexii8hj6lftvxguy KNI SOP]
* [https://caltech.box.com/s/9sx2vhd9gz5rdhviexii8hj6lftvxguy KNI SOP]
Line 46: Line 44:
===== Video Tutorials =====
===== Video Tutorials =====
* [https://youtu.be/jq5M7fkgpfM Labline Training]
* [https://youtu.be/jq5M7fkgpfM Labline Training]
* [https://youtu.be/5C6It9YO_jg Sample Load & Transfer]


== Specifications ==
== Specifications ==
Line 54: Line 53:
* Evaporation Source: 1x single emitter, 4-pocket e-beam evaporation source
* Evaporation Source: 1x single emitter, 4-pocket e-beam evaporation source
* 1x Argon ion source (Filament type)
* 1x Argon ion source (Filament type)
* Accepts up to 1x 150mm wafer or smaller wafers/pieces


== Related Instrumentation in the KNI ==
== Related Instrumentation in the KNI ==

Revision as of 23:24, 15 April 2024

Labline Evaporator
Instrument Type Deposition
Techniques E-beam Evaporation,
Ion-Assisted Deposition (IAD),
Ion Milling
Staff Manager Alex Wertheim
Staff Email alexw@caltech.edu
Staff Phone 626-395-3371
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B235C Steele
Lab Phone 626-395-1539
Manufacturer Kurt J. Lesker Company
Model Labline

Description

The Labline electron beam evaporator system is a load-locked platform with a cryopump for fast sample turnaround and a user-friendly interface for precise control of film parameters during deposition. It is fitted with a Kaufman and Robinson EH 400 End-Hall permanent magnet ion source that can be used for cleaning substrates and ion-assisted deposition during evaporation.

Applications
  • Metal deposition (Ti, Pt, Au, Al)
  • Lift-off
  • Non-selective etch
  • Ion-assisted deposition (simultaneous etching & deposition)

Resources

SOPs & Troubleshooting

Tool Reservation Rules

Advanced Reservation (days) Limit per Reservation (hrs) Limit per week (hrs)
Weekday 7 6 18
Weeknight 7 8 18
Weekend 7 12 18
Video Tutorials

Specifications

Hardware Specifications
  • Typical base pressure: 1E-7 to 1E-8 Torr
  • All dry pumping system (cryo & scroll pumps)
  • Load-lock-equipped system with manual wafer transfer
  • Evaporation Source: 1x single emitter, 4-pocket e-beam evaporation source
  • 1x Argon ion source (Filament type)
  • Accepts up to 1x 150mm wafer or smaller wafers/pieces