AJA Orion ATC Series Electron Beam Evaporator: Difference between revisions
Jump to navigation
Jump to search
No edit summary |
|||
| (7 intermediate revisions by 2 users not shown) | |||
| Line 2: | Line 2: | ||
|InstrumentName = AJA Orion ATC Series Electron Beam Evaporator | |InstrumentName = AJA Orion ATC Series Electron Beam Evaporator | ||
|HeaderColor = #F2682A | |HeaderColor = #F2682A | ||
|ImageOne = | |ImageOne = PXL 20230728 000709710 (1).jpg | ||
|ImageTwo = | |ImageTwo = | ||
|InstrumentType = [[Equipment_List#Deposition|Deposition]] | |InstrumentType = [[Equipment_List#Deposition|Deposition]] | ||
| Line 17: | Line 17: | ||
}} | }} | ||
== Description == | == Description == | ||
The AJA International ATC Orion Series system allows for | The AJA International ATC Orion Series system allows for electron beam evaporation of various metals, oxides, and semiconductors. This tool is a true UHV design equipped with dedicated heating jackets and internal heat lamps for an efficient bake-out process. A multi-crystal QCM protects against failed processes due to real-time thickness measurement errors and allows for long periods of maintained UHV conditions by removing the need to vent the chamber for regular sensor upkeep. In addition, crucibles may be swapped without breaking chamber vacuum via the use of a dedicated manual crucible exchanging system. | ||
===== Applications ===== | ===== Applications ===== | ||
* Metal deposition | * Metal deposition. Allows ferromagnetics and diamagnetics | ||
* Semiconductor deposition (in-situ doping not possible) | |||
* Oxide deposition | * Oxide deposition | ||
* Lift-off | * Lift-off | ||
== Resources == | == Resources == | ||
===== SOPs & Troubleshooting ===== | ===== SOPs & Troubleshooting ===== | ||
* [ | * [https://caltech.box.com/s/zygxa14nklirrtd6aw0fjdvqlggdyjh6 Standard Operating Procedures (SOP)] | ||
=== Tool Reservation Rules === | === Tool Reservation Rules === | ||
| Line 43: | Line 40: | ||
| Weekend || 7 || 12 || 18 | | Weekend || 7 || 12 || 18 | ||
|} | |} | ||
== Specifications == | == Specifications == | ||
| Line 68: | Line 61: | ||
===== Electron Beam Evaporation Systems ===== | ===== Electron Beam Evaporation Systems ===== | ||
* [[ | * [[Labline: Electron Beam Evaporator|Labline: Electron Beam Evaporator]] | ||
===== Chemical Vapor Deposition ===== | ===== Chemical Vapor Deposition ===== | ||
* [[FlexAL II: Atomic Layer Deposition (ALD)|FlexAL II: Atomic Layer Deposition (ALD)]] | * [[FlexAL II: Atomic Layer Deposition (ALD)|FlexAL II: Atomic Layer Deposition (ALD)]] | ||
* [[Plasma-Enhanced Chemical Vapor Deposition (PECVD)|Plasma-Enhanced Chemical Vapor Deposition (PECVD)]] | * [[Plasma-Enhanced Chemical Vapor Deposition (PECVD)|Plasma-Enhanced Chemical Vapor Deposition (PECVD)]] | ||
Latest revision as of 19:28, 19 March 2026
|
Description
The AJA International ATC Orion Series system allows for electron beam evaporation of various metals, oxides, and semiconductors. This tool is a true UHV design equipped with dedicated heating jackets and internal heat lamps for an efficient bake-out process. A multi-crystal QCM protects against failed processes due to real-time thickness measurement errors and allows for long periods of maintained UHV conditions by removing the need to vent the chamber for regular sensor upkeep. In addition, crucibles may be swapped without breaking chamber vacuum via the use of a dedicated manual crucible exchanging system.
Applications
- Metal deposition. Allows ferromagnetics and diamagnetics
- Semiconductor deposition (in-situ doping not possible)
- Oxide deposition
- Lift-off
Resources
SOPs & Troubleshooting
Tool Reservation Rules
| Advanced Reservation (days) | Limit per Reservation (hrs) | Limit per week (hrs) | |
|---|---|---|---|
| Weekday | 7 | 6 | 18 |
| Weeknight | 7 | 8 | 18 |
| Weekend | 7 | 12 | 18 |
Specifications
Hardware Specifications
- Typical base pressure: <5E-9 Torr
- All dry pumping system (cryo & scroll pumps)
- Load-lock-equipped system with automatic wafer transfer
- Evaporation Source: 1x single emitter, 6-pocket e-beam evaporation source
- Pockets 1-4 allow in-situ crucible exchange through dedicated secondary load lock, allowing for crucible swap without breaking UHV chamber conditions.
- Accepts up to 1x 150mm wafer or smaller wafers/pieces
- Optional lift-off dome holds 4x 100mm wafers for batch processing
- Camera for E-Beam/Crucible observation during process
- Inficon CrystalSix(TM)
- 6-crystal QCM with automatic crystal switching in event of crystal fail or low Q. Enables long periods of maintained UHV conditions without requiring venting to exchange crystals
- Programmable deposition processes
