|InstrumentName = AJA Orion ATC Series Electron Beam Evaporator
|InstrumentName = AJA Orion ATC Series Electron Beam Evaporator
|HeaderColor = #F2682A
|HeaderColor = #F2682A
|ImageOne =  
|ImageOne = PXL 20230728 000709710 (1).jpg
|ImageTwo =  
|ImageTwo =  
|InstrumentType = [[Equipment_List#Deposition|Deposition]]
|InstrumentType = [[Equipment_List#Deposition|Deposition]]
Line 17: Line 17:
}}
}}
== Description ==
== Description ==
The AJA International ATC Orion Series system allows for programmable evaporation processes and a convenient ease of maintaining.  
The AJA International ATC Orion Series system allows for electron beam evaporation of various metals, oxides, and semiconductors. This tool is a true UHV design equipped with dedicated heating jackets and internal heat lamps for an efficient bake-out process. A multi-crystal QCM protects against failed processes due to real-time thickness measurement errors and allows for long periods of maintained UHV conditions by removing the need to vent the chamber for regular sensor upkeep. In addition, crucibles may be swapped without breaking chamber vacuum via the use of a dedicated manual crucible exchanging system.  


===== Applications =====
===== Applications =====
* Metal deposition
* Metal deposition
* Semiconductor deposition (in-situ doping not possible)
* Oxide deposition
* Oxide deposition
* Lift-off
* Lift-off


== Resources ==
== Resources ==
===== Equipment Status =====
* [https://labrunr.caltech.edu/Equipment_2.aspx LabRunr Equipment Status] (Select AJA Orion E-Beam Evaporator from the dropdown menu)
===== SOPs & Troubleshooting =====
===== SOPs & Troubleshooting =====
* [linkgoeshere Standard Operating Procedures (SOP)]
* [https://caltech.box.com/s/zygxa14nklirrtd6aw0fjdvqlggdyjh6 Standard Operating Procedures (SOP)]
* [linkgoeshere Troubleshooting Guide]


=== Tool Reservation Rules ===
=== Tool Reservation Rules ===
Line 43: Line 40:
| Weekend || 7 || 12 || 18
| Weekend || 7 || 12 || 18
|}
|}
===== Video Tutorials =====
* [linkgoeshere General System Operation]
* [linkgoeshere In-Situ Crucible Exchange]


== Specifications ==
== Specifications ==
Line 68: Line 61:


===== Electron Beam Evaporation Systems =====
===== Electron Beam Evaporation Systems =====
* [[CHA: Electron Beam Evaporator|CHA: Electron Beam Evaporator]]
* [[Labline: Electron Beam Evaporator|Labline: Electron Beam Evaporator]]


===== Chemical Vapor Deposition =====
===== Chemical Vapor Deposition =====
* [[FlexAL II: Atomic Layer Deposition (ALD)|FlexAL II: Atomic Layer Deposition (ALD)]]
* [[FlexAL II: Atomic Layer Deposition (ALD)|FlexAL II: Atomic Layer Deposition (ALD)]]
* [[Plasma-Enhanced Chemical Vapor Deposition (PECVD)|Plasma-Enhanced Chemical Vapor Deposition (PECVD)]]
* [[Plasma-Enhanced Chemical Vapor Deposition (PECVD)|Plasma-Enhanced Chemical Vapor Deposition (PECVD)]]

Revision as of 00:47, 26 April 2024

AJA Orion ATC Series Electron Beam Evaporator
Instrument Type Deposition
Techniques E-beam Evaporation
Staff Manager Alex Wertheim
Staff Email alexw@caltech.edu
Staff Phone 626-395-3371
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B235C Steele
Lab Phone 626-395-1539
Manufacturer AJA International
Model ATC Orion

Description

The AJA International ATC Orion Series system allows for electron beam evaporation of various metals, oxides, and semiconductors. This tool is a true UHV design equipped with dedicated heating jackets and internal heat lamps for an efficient bake-out process. A multi-crystal QCM protects against failed processes due to real-time thickness measurement errors and allows for long periods of maintained UHV conditions by removing the need to vent the chamber for regular sensor upkeep. In addition, crucibles may be swapped without breaking chamber vacuum via the use of a dedicated manual crucible exchanging system.

Applications
  • Metal deposition
  • Semiconductor deposition (in-situ doping not possible)
  • Oxide deposition
  • Lift-off

Resources

SOPs & Troubleshooting

Tool Reservation Rules

Advanced Reservation (days) Limit per Reservation (hrs) Limit per week (hrs)
Weekday 7 6 18
Weeknight 7 8 18
Weekend 7 12 18

Specifications

Hardware Specifications
  • Typical base pressure: <5E-9 Torr
  • All dry pumping system (cryo & scroll pumps)
  • Load-lock-equipped system with automatic wafer transfer
  • Evaporation Source: 1x single emitter, 6-pocket e-beam evaporation source
    • Pockets 1-4 allow in-situ crucible exchange through dedicated secondary load lock, allowing for crucible swap without breaking UHV chamber conditions.
  • Accepts up to 1x 150mm wafer or smaller wafers/pieces
  • Optional lift-off dome holds 4x 100mm wafers for batch processing
  • Camera for E-Beam/Crucible observation during process
  • Inficon CrystalSix(TM)
    • 6-crystal QCM with automatic crystal switching in event of crystal fail or low Q. Enables long periods of maintained UHV conditions without requiring venting to exchange crystals
  • Programmable deposition processes
Sputtering Systems
Electron Beam Evaporation Systems
Chemical Vapor Deposition