EBPG 5200: 100 kV Electron Beam Lithography: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
Line 29: Line 29:
== Resources ==
== Resources ==
===== General SOPs =====
===== General SOPs =====
* [https://caltech.box.com/s/95dcyqt1vij9bmkdjui4jqz4qe9jzqmn EBPG reservation and use policy (COVID-19 Updates)]
* [https://caltech.box.com/s/qzhf1h1su3a1vadl6p76mg6tav49uisn EBPG SOP]
* [https://caltech.box.com/s/qzhf1h1su3a1vadl6p76mg6tav49uisn EBPG SOP]
* [https://caltech.box.com/s/jq0s85sdsd069cv9aesdfixy5fueihyh User's Guide to the EBPG pg computer desktop]
* [https://caltech.box.com/s/jq0s85sdsd069cv9aesdfixy5fueihyh User's Guide to the EBPG pg computer desktop]
* [https://caltech.box.com/s/9whswv26y0w6yua8073nw080r3lcfdz4 EBPG Troubleshooting Guide]
* [https://caltech.box.com/s/9whswv26y0w6yua8073nw080r3lcfdz4 EBPG Troubleshooting Guide]
* [https://caltech.box.com/s/cwp88iw2q5t8eygl114zs8ywlhraxo16 EBPG reservation and use policy]
* [https://caltech.box.com/s/cwp88iw2q5t8eygl114zs8ywlhraxo16 EBPG reservation and use policy (Legacy version)]
* [https://caltech.box.com/s/s21wk4nw02qmbugt4z30zjbold5sz41p EBPG Training presentation (Caltech-only access)]
* [https://caltech.box.com/s/s21wk4nw02qmbugt4z30zjbold5sz41p EBPG Training presentation (Caltech-only access)]
* [https://caltech.box.com/s/qkd3gkrmcd3c4ze2xliabt00lhisj5zy EBPG Pre-exposure Walkthrough procedure (video)]
* [https://caltech.box.com/s/qkd3gkrmcd3c4ze2xliabt00lhisj5zy EBPG Pre-exposure Walkthrough procedure (video)]

Revision as of 21:03, 15 June 2020

EBPG 5200
Wavelength-scale-Piezoelectric-Transducer Alp-Sipahigil.jpg
Instrument Type Lithography
Techniques Electron Beam Lithography
Staff Manager Guy A. DeRose, PhD
Staff Email derose@caltech.edu
Staff Phone 626-395-3423
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B233C Steele
Lab Phone 626-395-1531 & -1540
Manufacturer Raith Lithography BV
Model EBPG 5200
EBPG-5200.jpg

Description

The Raith EBPG 5200 is a dedicated direct-write Electron Beam Pattern Generator that is used to pattern large areas by high-resolution electron beam lithography. This instrument has substrate holders to handle 3" wafers, piece parts from a couple of mm to 3" diameter and up to 6.35 mm thick, and 6" mask plates. This instrument can be outfitted with substrate holders to handle up to 200 mm wafers. While this instrument can be set to operate at 20, 50, or 100 keV, it is normally set for 100 keV operation (i.e. with an accelerating voltage of 100 kV, the average energy per electron is 100 keV).

Operational Applications
  • Non-aligned electron beam lithography
  • Aligned (aka direct-write) electron beam lithography
Scientific / Technical Applications
  • Nanophotonics
  • Nano-optics
  • Waveguides

Resources

General SOPs
Sample Prep and Writing SOPs
Troubleshooting SOPs
Data Preparation Resources
Lithography Process Information
Manufacturer Manuals

Specifications

  • Voltage Range: 20, 50 or 100 kV
  • Current Range: 50 pA to 200 nA
  • Main Field Size: Up to 1 mm x 1 mm
  • Main Field Resolution: 20 bit
  • Maximum Writing Frequency: 100 MHz
  • Aperture Sizes: 200 μm, 300 μm, 400 μm