EBPG 5000+: 100 kV Electron Beam Lithography: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
Derose (talk | contribs)
Derose (talk | contribs)
Line 58: Line 58:
* [https://caltech.box.com/s/emfc1i4qeg9psatj6enpm9g38f5a2u9r EBPG FEG recovery and new beam table SOP]
* [https://caltech.box.com/s/emfc1i4qeg9psatj6enpm9g38f5a2u9r EBPG FEG recovery and new beam table SOP]
* [https://caltech.box.com/s/oxjf52qwvj0ocnx151aqd6tso8ykfkca Raith Common errors and solutions with aligned writing SOP]
* [https://caltech.box.com/s/oxjf52qwvj0ocnx151aqd6tso8ykfkca Raith Common errors and solutions with aligned writing SOP]
* [https://caltech.box.com/s/1ge5czbz4b1pbfz2wrzbjmynnktdc0ci EBPG 5000+ Troubleshooting Loader errors]


===== Data Preparation Resources =====
===== Data Preparation Resources =====

Revision as of 06:19, 6 February 2020

EBPG 5000+
Instrument Type Lithography
Techniques Electron Beam Lithography
Staff Manager Guy A. DeRose, PhD
Staff Email derose@caltech.edu
Staff Phone 626-395-3423
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B233C Steele
Lab Phone 626-395-1531 & -1540
Manufacturer Raith Lithography BV
Model EBPG 5000+

Description

The Raith EBPG 5000+ is a dedicated direct-write Electron Beam Pattern Generator that is used to pattern large areas by high-resolution electron beam lithography. This instrument has substrate holders to handle 2, 4, and 6" wafers, piece parts from a couple of mm to 6" diameter, and 3" and 5" mask plates. While this instrument can be set to operate at 20, 50, or 100 keV, it is normally set for 100 keV operation (i.e. with an accelerating voltage of 100 kV, the average energy per electron is 100 keV).

Operational Applications
  • Non-aligned electron beam lithography
  • Aligned (aka direct-write) electron beam lithography
Scientific / Technical Applications
  • Nanophotonics
  • Nano-optics
  • Waveguides

Resources

General SOPs
Sample Prep and Writing SOPs
Troubleshooting SOPs
Data Preparation Resources
Lithography Process Information
Manufacturer Manuals

Specifications

Manufacturer Specifications and Manuals
Specifications
  • Voltage Range: 20, 50 or 100 kV
  • Current Range: 50 pA to 200 nA
  • Main Field Size: Up to 1 mm x 1 mm
  • Main Field Resolution: 20 bit
  • Maximum Writing Frequency: 100 MHz
  • Aperture Sizes: 300μm, 300μm, 400μm



Electron Beam Lithography
Ion Beam Lithography