EBPG 5200: 100 kV Electron Beam Lithography: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
Derose (talk | contribs)
Derose (talk | contribs)
Line 61: Line 61:
===== Advanced Troubleshooting SOPs =====
===== Advanced Troubleshooting SOPs =====
* [https://caltech.box.com/s/55zji9vfs8kuxl0aye1sw1iy8xi0rd9c Information Archive Beam]
* [https://caltech.box.com/s/55zji9vfs8kuxl0aye1sw1iy8xi0rd9c Information Archive Beam]
* [https://caltech.box.com/s/qr7lqvsjc7cgv471f33smyn6gqjzdqfr EBPG BEAMS crash recovery SOP (run before a coldstart if BEAMS freezes)]
* [https://caltech.box.com/s/qnl5l52v936kql830kt0fyrmlaj8cbmo BEAMS $pg shutdown / coldstart SOP]
* [https://caltech.box.com/s/qnl5l52v936kql830kt0fyrmlaj8cbmo BEAMS $pg shutdown / coldstart SOP]
* [https://caltech.box.com/s/et1ak4l0t7cwermp3h51w1aolywe09vr EBPG Procedure to degauss the final lens (run after every coldstart)]
* [https://caltech.box.com/s/et1ak4l0t7cwermp3h51w1aolywe09vr EBPG Procedure to degauss the final lens (run after every coldstart)]

Revision as of 22:24, 24 September 2020

EBPG 5200
Instrument Type Lithography
Techniques Electron Beam Lithography
Staff Manager Guy A. DeRose, PhD
Staff Email derose@caltech.edu
Staff Phone 626-395-3423
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B233C Steele
Lab Phone 626-395-1531 & -1540
Manufacturer Raith Lithography BV
Model EBPG 5200

Description

The Raith EBPG 5200 is a dedicated direct-write Electron Beam Pattern Generator that is used to pattern large areas by high-resolution electron beam lithography. This instrument has substrate holders to handle 3" wafers, piece parts from a couple of mm to 3" diameter and up to 6.35 mm thick, and 6" mask plates. This instrument can be outfitted with substrate holders to handle up to 200 mm wafers. While this instrument can be set to operate at 20, 50, or 100 keV, it is normally set for 100 keV operation (i.e. with an accelerating voltage of 100 kV, the average energy per electron is 100 keV).

Operational Applications
  • Non-aligned electron beam lithography
  • Aligned (aka direct-write) electron beam lithography
Scientific / Technical Applications
  • Nanophotonics
  • Nano-optics
  • Waveguides

Resources

Equipment Data
General SOPs
Training Materials
Sample Prep and Writing SOPs
Advanced Troubleshooting SOPs
Data Preparation Resources
Lithography Process Information
Manufacturer Manuals

Specifications

  • Voltage Range: 20, 50 or 100 kV
  • Current Range: 50 pA to 200 nA
  • Main Field Size: Up to 1 mm x 1 mm
  • Main Field Resolution: 20 bit
  • Maximum Writing Frequency: 100 MHz
  • Aperture Sizes: 200 μm, 300 μm, 400 μm