EBPG 5200: 100 kV Electron Beam Lithography: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
Line 30: Line 30:
===== Equipment Data =====
===== Equipment Data =====
* [https://caltech.box.com/s/j19tuhv68bk0nsa5nruc95g4dizzxtr7 EBPG Pass-down equipment information]
* [https://caltech.box.com/s/j19tuhv68bk0nsa5nruc95g4dizzxtr7 EBPG Pass-down equipment information]
===== General SOPs =====
===== General SOPs =====
* [https://caltech.box.com/s/95dcyqt1vij9bmkdjui4jqz4qe9jzqmn EBPG reservation and use policy (COVID-19 Updates)]
* [https://caltech.box.com/s/95dcyqt1vij9bmkdjui4jqz4qe9jzqmn EBPG reservation and use policy (COVID-19 Updates)]
Line 38: Line 39:
* [https://caltech.box.com/s/s21wk4nw02qmbugt4z30zjbold5sz41p EBPG Training presentation (Caltech-only access)]
* [https://caltech.box.com/s/s21wk4nw02qmbugt4z30zjbold5sz41p EBPG Training presentation (Caltech-only access)]
* [https://caltech.box.com/s/qkd3gkrmcd3c4ze2xliabt00lhisj5zy EBPG Pre-exposure Walkthrough procedure (video)]
* [https://caltech.box.com/s/qkd3gkrmcd3c4ze2xliabt00lhisj5zy EBPG Pre-exposure Walkthrough procedure (video)]
* [https://caltech.box.com/s/4h37s09pg1lc2khlwjc67z95qlooa6az EBPG System Introduction main room (training video)]
* [https://caltech.box.com/s/fd9wzhdt2a0qmkgcwerqd27lvi26ca8x EBPG System Introduction service chase overview (training video)]
* [https://caltech.box.com/s/ykm83f8maelbqb65140rd6607hayjwa9 EBPG System Introduction UPS and alignment microscopes (training video)]


===== Sample Prep and Writing SOPs =====
===== Sample Prep and Writing SOPs =====

Revision as of 18:51, 10 August 2020

EBPG 5200
Wavelength-scale-Piezoelectric-Transducer Alp-Sipahigil.jpg
Instrument Type Lithography
Techniques Electron Beam Lithography
Staff Manager Guy A. DeRose, PhD
Staff Email derose@caltech.edu
Staff Phone 626-395-3423
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B233C Steele
Lab Phone 626-395-1531 & -1540
Manufacturer Raith Lithography BV
Model EBPG 5200
EBPG-5200.jpg

Description

The Raith EBPG 5200 is a dedicated direct-write Electron Beam Pattern Generator that is used to pattern large areas by high-resolution electron beam lithography. This instrument has substrate holders to handle 3" wafers, piece parts from a couple of mm to 3" diameter and up to 6.35 mm thick, and 6" mask plates. This instrument can be outfitted with substrate holders to handle up to 200 mm wafers. While this instrument can be set to operate at 20, 50, or 100 keV, it is normally set for 100 keV operation (i.e. with an accelerating voltage of 100 kV, the average energy per electron is 100 keV).

Operational Applications
  • Non-aligned electron beam lithography
  • Aligned (aka direct-write) electron beam lithography
Scientific / Technical Applications
  • Nanophotonics
  • Nano-optics
  • Waveguides

Resources

Equipment Data
General SOPs
Sample Prep and Writing SOPs
Troubleshooting SOPs
Data Preparation Resources
Lithography Process Information
Manufacturer Manuals

Specifications

  • Voltage Range: 20, 50 or 100 kV
  • Current Range: 50 pA to 200 nA
  • Main Field Size: Up to 1 mm x 1 mm
  • Main Field Resolution: 20 bit
  • Maximum Writing Frequency: 100 MHz
  • Aperture Sizes: 200 μm, 300 μm, 400 μm