ICP-RIE: Dielectric Etcher: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
Derose (talk | contribs)
Derose (talk | contribs)
Line 65: Line 65:
== Specifications ==
== Specifications ==
===== Manufacturer Specifications =====
===== Manufacturer Specifications =====
* [https://caltech.box.com/s/nmws6w7643ne8mraljjar6c4epw0anpp Manufacturer Data Sheet]
* [https://caltech.box.com/s/85mj9roas98jtwee9d22hk0wk9un54fl Manufacturer System Configuration]
 
===== Mode 1 Specifications =====
===== Mode 1 Specifications =====
* Voltage Range: 0.5 to 30.0 kV
* Voltage Range: 0.5 to 30.0 kV

Revision as of 15:29, 22 May 2019

Dielectric Etcher
Instrument Type Etching
Techniques pseudoBosch
Cryogenic silicon etch
Staff Manager Nathan S. Lee
Staff Email nathslee@caltech.edu
Staff Phone 626-395-1319
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B235 Steele
Lab Phone 626-395-1532
Manufacturer Oxford Instruments
Model {{{Model}}}

Description

The Dielectric Inductively Coupled Plasma - Reactive Ion Etch (ICP-RIE) is an Oxford Instruments Plasma Technology Plasmalab System 100 ICP-RIE 380 system that is optimized for silicon etching. This system is configured for silicon etching with "pseudoBosch" C4F8 and SF6 gases, and cryogenic silicon etch with SF6 and O2. The silicon ICP-RIE has a variable temperature stage (-150 to 400 °C). This system supports wafer sizes up to 6 inches, and provides accurate deep etching capabilities for silicon and "silicon-like" samples only.

Applications
  • Cryogenic etch of silicon
  • pseudo-Bosch of silicon
Allowed material in Dielectric Etch System
  • Si, SixNy, SiO2
  • PMMA/ZEP/SPR/AZ/maN resists, SiOx/Al2O3 hard masks
  • No metals
Dielectric Etcher Gas List
  • SF6
  • C4F8
  • O2
  • Ar
  • N2
  • CHF3
  • N2O
  • NH3

Resources

SOPs & Troubleshooting
Process Documents
Video Tutorials
Graphical Handouts
Presentations
Manufacturer Manuals

Specifications

Manufacturer Specifications
Mode 1 Specifications
  • Voltage Range: 0.5 to 30.0 kV
  • Aperture Sizes: 10 mm, 15 mm, 20 mmm, 30 mm
  • etc.
Mode 2 Specifications
  • Voltage Range: 5.0 to 30.0 kV
  • Current Range: 10 pA - 20 nA
  • etc.