Rapid Thermal Processor: Difference between revisions
Jump to navigation
Jump to search
No edit summary |
|||
| (17 intermediate revisions by 4 users not shown) | |||
| Line 7: | Line 7: | ||
|RoomLocation = B235 Steele | |RoomLocation = B235 Steele | ||
|LabPhone = 626-395-1539 | |LabPhone = 626-395-1539 | ||
|PrimaryStaff = [[ | |PrimaryStaff = [[Alex Wertheim]] | ||
|StaffEmail = | |StaffEmail = alexw@caltech.edu | ||
|StaffPhone = 626-395- | |StaffPhone = 626-395-3371 | ||
|Manufacturer = Surface | |Manufacturer = Surface Science Integration | ||
|Model = Solaris 150 | |Model = Solaris 150 | ||
|Techniques = Rapid Thermal Processing | |Techniques = Rapid Thermal Processing | ||
|RequestTraining = | |RequestTraining = alexw@caltech.edu | ||
|EmailList = kni-metrology | |EmailList = kni-metrology | ||
|EmailListName = Metrology | |EmailListName = Metrology | ||
}} | }} | ||
== Description == | == Description == | ||
The Solaris 150 is a manual loading Rapid Thermal Processor system that can process up to 6 inch substrates. The | The Solaris 150 is a manual loading Rapid Thermal Processor system that can process up to 6 inch substrates. The system is designed for silicon implant annealing and monitoring and compound semiconductor implant activation and ohmic alloying. | ||
===== Applications ===== | ===== Applications ===== | ||
*Temperature range from room temperature to 1200 degrees C. | *Temperature range from room temperature to 1200 degrees C. | ||
* Processing gasses available: | * Processing gasses available: | ||
**Nitrogen | **Nitrogen | ||
**Forming Gas | **Argon | ||
**Forming Gas (5% H2 in N2) | |||
== Resources == | == Resources == | ||
===== SOPs ===== | ===== SOPs ===== | ||
* SOP | *[https://caltech.box.com/s/9less1mp9tg7xya8ugycnw11dhw0lnjf Solaris 150 – Rapid Thermal Processor -Short SOP] | ||
*[https://caltech.box.com/s/7uozrq6pmgkcr6l8u3qhnka9sgtgf3u9 Solaris 150 – Rapid Thermal Processor -Long SOP] | |||
===== Manuals ===== | |||
*[https://caltech.app.box.com/file/1237887943601 Solaris 150 - Rapid Thermal Processor Manual] | |||
<br> | <br> | ||
<br> | <br> | ||
Latest revision as of 23:10, 24 September 2025
|
Description
The Solaris 150 is a manual loading Rapid Thermal Processor system that can process up to 6 inch substrates. The system is designed for silicon implant annealing and monitoring and compound semiconductor implant activation and ohmic alloying.
Applications
- Temperature range from room temperature to 1200 degrees C.
- Processing gasses available:
- Nitrogen
- Argon
- Forming Gas (5% H2 in N2)