XeF2 Etcher for Silicon: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
Derose (talk | contribs)
No edit summary
 
(3 intermediate revisions by 2 users not shown)
Line 13: Line 13:
|Model = N/A
|Model = N/A
|Techniques = Selective dry Si etching
|Techniques = Selective dry Si etching
|RequestTraining = alexw@caltech.edu
|RequestTraining = kmmckenz@caltech.edu
|EmailList = kni-XeF2
|EmailList = kni-XeF2
|EmailListName = XeF<sub>2</sub>
|EmailListName = XeF<sub>2</sub>
Line 25: Line 25:


== Resources ==
== Resources ==
===== Equipment Status =====
* [https://labrunr.caltech.edu/Equipment_2.aspx LabRunr Equipment Status] (Select XeF2 from the dropdown menu)
===== SOPs =====
===== SOPs =====
* [https://caltech.box.com/s/2zf5dwmdjyjxptvoscxkxe6yt57vr85v KNI SOP]
* [https://caltech.box.com/s/2zf5dwmdjyjxptvoscxkxe6yt57vr85v KNI SOP]

Latest revision as of 18:42, 8 October 2025

XeF2 Silicon Etcher
Instrument Type Etching
Techniques Selective dry Si etching
Staff Manager Alex Wertheim
Staff Email alexw@caltech.edu
Staff Phone 626-395-3371
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B235C Steele
Lab Phone 626-395-1539
Manufacturer N/A
Model N/A

Description

The XeF2 etcher flows pressure- and time-controlled pulses of XeF2 gas into a chamber to deliver an isotropic etch that is highly selective only to silicon. It is commonly used to remove Si under layers that are accessed through vias, in order to suspend membranes and other structures in MEMS devices.

Applications
  • Very high selectivity dry Si etching
  • MEMS fabrication

Resources

SOPs