XeF2 Etcher for Silicon: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
mNo edit summary
Derose (talk | contribs)
(4 intermediate revisions by 3 users not shown)
Line 1: Line 1:
{{InstrumentInfoboxOneImage|
{{InstrumentInfoboxOneImage|
|InstrumentName = XeF<sub>2</sub> Silicon Etcher  
|InstrumentName = XeF<sub>2</sub> Silicon Etcher  
|HeaderColor = #F5A81C
|HeaderColor = #FFE2B9
|ImageOne = XeF2-Etcher.jpg
|ImageOne = XeF2-Etcher.jpg
|ImageTwo =  
|ImageTwo =  
|InstrumentType = [[Equipment_List#Etching|Etching]]
|InstrumentType = [[Equipment_List#Etching|Etching]]
|RoomLocation =  
|RoomLocation = B235C Steele
|LabPhone = 626-395-1539
|LabPhone = 626-395-1539
|PrimaryStaff = [[Alex Wertheim]]
|PrimaryStaff = [[Alex Wertheim]]
Line 14: Line 14:
|Techniques = Selective dry Si etching
|Techniques = Selective dry Si etching
|RequestTraining = alexw@caltech.edu
|RequestTraining = alexw@caltech.edu
|EmailList = kni-XeF2@caltech.edu
|EmailList = kni-XeF2
|EmailListName = XeF<sub>2</sub>
|EmailListName = XeF<sub>2</sub>
}}
}}
== Description ==
== Description ==
The XeF<sub>2</sub> etcher flows pressure and time controlled pulses of XeF<sub>2</sub> gas into a chamber to deliver an isotropic etch which is highly selective only to Silicon. It is commonly used to remove Si under layers accessed through Vias to suspend membranes and other structures in MEMS devices.  
The XeF<sub>2</sub> etcher flows pressure- and time-controlled pulses of XeF<sub>2</sub> gas into a chamber to deliver an isotropic etch that is highly selective only to silicon. It is commonly used to remove Si under layers that are accessed through vias, in order to suspend membranes and other structures in MEMS devices.  


===== Applications =====
===== Applications =====
Line 25: Line 25:


== Resources ==
== Resources ==
===== Equipment Status =====
* [https://labrunr.caltech.edu/Equipment_2.aspx LabRunr Equipment Status] (Select XeF2 from the dropdown menu)
===== SOPs =====
===== SOPs =====
* [https://caltech.box.com/s/2zf5dwmdjyjxptvoscxkxe6yt57vr85v KNI SOP]
* [https://caltech.box.com/s/2zf5dwmdjyjxptvoscxkxe6yt57vr85v KNI SOP]

Revision as of 05:33, 30 June 2022

XeF2 Silicon Etcher
Instrument Type Etching
Techniques Selective dry Si etching
Staff Manager Alex Wertheim
Staff Email alexw@caltech.edu
Staff Phone 626-395-3371
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B235C Steele
Lab Phone 626-395-1539
Manufacturer N/A
Model N/A

Description

The XeF2 etcher flows pressure- and time-controlled pulses of XeF2 gas into a chamber to deliver an isotropic etch that is highly selective only to silicon. It is commonly used to remove Si under layers that are accessed through vias, in order to suspend membranes and other structures in MEMS devices.

Applications
  • Very high selectivity dry Si etching
  • MEMS fabrication