Difference between revisions of "EBPG 5000+: 100 kV Electron Beam Lithography"

From the KNI Lab at Caltech
Jump to navigation Jump to search
Line 36: Line 36:
* [https://caltech.box.com/s/jq0s85sdsd069cv9aesdfixy5fueihyh User's Guide to the EBPG pg computer desktop]
* [https://caltech.box.com/s/jq0s85sdsd069cv9aesdfixy5fueihyh User's Guide to the EBPG pg computer desktop]
* [https://caltech.box.com/s/9whswv26y0w6yua8073nw080r3lcfdz4 EBPG Troubleshooting Guide]
* [https://caltech.box.com/s/9whswv26y0w6yua8073nw080r3lcfdz4 EBPG Troubleshooting Guide]
* [https://caltech.box.com/s/cwp88iw2q5t8eygl114zs8ywlhraxo16 EBPG reservation and use policy (Legacy version)]
* [https://caltech.box.com/s/cf5ix7iraea7m3jepjwylf4nd51d8hrg Remote EBPG access via HP Remote Graphics Server (Caltech-Only)]
* [https://caltech.box.com/s/cf5ix7iraea7m3jepjwylf4nd51d8hrg Remote EBPG access via HP Remote Graphics Server (Caltech-Only)]



Revision as of 18:51, 13 May 2022

EBPG 5000+
EBPG-5000+.jpg
Instrument Type Lithography
Techniques Electron Beam Lithography
Staff Manager Guy A. DeRose, PhD
Staff Email derose@caltech.edu
Staff Phone 626-395-3423
Reserve time on LabRunr
Request training by email
Sign up for EBPG email list
Lab Location B233C Steele
Lab Phone 626-395-1531 & -1540
Manufacturer Raith Lithography BV
Model EBPG 5000+

Description

The Raith EBPG 5000+ is a dedicated direct-write Electron Beam Pattern Generator that is used to pattern large areas by high-resolution electron beam lithography. This instrument has substrate holders to handle 2, 4, and 6" wafers, piece parts from a couple of mm to 6" diameter, and 3" and 5" mask plates. While this instrument can be set to operate at 20, 50, or 100 keV, it is normally set for 100 keV operation (i.e. with an accelerating voltage of 100 kV, the average energy per electron is 100 keV).

Operational Applications
  • Non-aligned electron beam lithography
  • Aligned (aka direct-write) electron beam lithography
Scientific / Technical Applications
  • Nanophotonics
  • Nano-optics
  • Waveguides

Resources

Equipment Data
General SOPs
Training materials
Sample Prep and Writing SOPs
Advanced Troubleshooting SOPs
Data Preparation Resources
Lithography Process Information
Manufacturer Manuals

Specifications

Manufacturer Specifications and Manuals
Specifications
  • Voltage Range: 20, 50 or 100 kV
  • Current Range: 50 pA to 200 nA
  • Main Field Size: Up to 1 mm x 1 mm
  • Main Field Resolution: 20 bit
  • Maximum Writing Frequency: 100 MHz
  • Aperture Sizes: 300μm, 300μm, 400μm



Related Instrumentation in the KNI

Electron Beam Lithography
Ion Beam Lithography