Tube Furnaces for Wet & Dry Processing
|
Description
The system is designed for processing up to one-hundred, 150 mm (6") wafers per tube. Tube 1 is designated for wet & dry oxidation using a flask evaporator. Tube 2 is designated for dry oxidation and annealing.
Applications
- Dry & Wet oxidation
- Annealing