The Raith EBPG 5200 is a dedicated direct-write Electron Beam Pattern Generator that is used to pattern large areas by high resolution electron beam lithography. This instrument has substrate holders to handle 3" wafers, piece parts from a couple of mm to 3" diameter and up to 6.35mm thick, and 6" mask plates. This instrument can be outfitted with substrate holders to handle up to 200mm wafers. While this instrument can be set to operate at 20, 50, or 100 keV, it is normally set for 100 keV operation.
Opertional Applications
Non-aligned electron beam lithography
Aligned (AKA direct-write) electron beam lithography