DWL-66: Direct-Write Laser System: Difference between revisions
Jump to navigation
Jump to search
| Line 23: | Line 23: | ||
== Resources == | == Resources == | ||
===== Equipment Data ===== | |||
* [https://caltech.box.com/s/j19tuhv68bk0nsa5nruc95g4dizzxtr7 Lithography Pass-down equipment information] | |||
===== SOPs ===== | ===== SOPs ===== | ||
* [https://caltech.box.com/s/y86tagq2ajxt16wnj5bmqwupas1f1bs7 Operation SOP] | * [https://caltech.box.com/s/y86tagq2ajxt16wnj5bmqwupas1f1bs7 Operation SOP] | ||
Revision as of 04:03, 1 August 2020
|
Description
The Heidelberg Instruments DWL-66 is a tool for mask making and for direct patterning of wafers by the use of a HeCd laser. Precise control of the laser head and alignment produces 800-nm resolution lithography. The DWL 66 is an extremely high-resolution imaging system where over half a million dpi (dots per inch) is achieved using a 40-nm writeable address grid for exposing chrome plates or wafers.
Applications
- Direct Writing
- Grayscale Writing
Resources
Equipment Data
SOPs
Optical Lithography Resources
Manufacturer Manuals
Specifications
- Exposure: 442 nm wavelength HeCd laser