Revision as of 00:07, 20 May 2019
|
Description
The SB6L wafer bonder applies force and heat to the back side of two wafers in a vacuum chamber to bond them face to face. An automatic recipe can be created with control over bonding pressure, temperature, and chamber pressure as well as ramp/duration of any process step. Since heat and temperature can be controlled separately, temperature sensitive materials such as polymers may be bonded.
Applications
- MEMS & Microelectronics fabrication