Parylene Coater: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
Created page with "{{InstrumentInfoboxOneImage| |InstrumentName = Para Tech LabTop 3000 Parylene Coater |HeaderColor = #F5A81C |ImageOne = LabTop-3000-Parylene-Coater.jpg |ImageTwo = |Instrumen..."
 
No edit summary
 
(5 intermediate revisions by 3 users not shown)
Line 1: Line 1:
{{InstrumentInfoboxOneImage|
{{InstrumentInfoboxOneImage|
|InstrumentName = Para Tech LabTop 3000 Parylene Coater
|InstrumentName = Parylene Coater
|HeaderColor = #F5A81C
|HeaderColor = #F2682A
|ImageOne = LabTop-3000-Parylene-Coater.jpg
|ImageOne = LabTop-3000-Parylene-Coater.jpg
|ImageTwo =  
|ImageTwo =  
|InstrumentType = [[Equipment_List#Deposition|Deposition]]
|InstrumentType = [[Equipment_List#Deposition|Deposition]]
|RoomLocation =  
|RoomLocation = B203 Steele
|LabPhone = 626-395-1539
|LabPhone = 626-395-1539
|PrimaryStaff = [[Alex Wertheim]]
|PrimaryStaff = [[Nathan S. Lee]]
|StaffEmail = alexw@caltech.edu
|StaffEmail = nathslee@caltech.edu
|StaffPhone = 626-395-3371
|StaffPhone = 626-395-4386
|Manufacturer = Para Tech
|Manufacturer = Para Tech
|Techniques = Parylene deposition
|Model = LabTop 3000
|RequestTraining = alexw@caltech.edu
|Techniques = Parylene Deposition
|EmailList = kni-parylene@caltech.edu
|RequestTraining = Alexw@caltech.edu
|EmailListName = kni-parylene
|EmailList = kni-parylene
|EmailListName = Parylene
}}
}}
== Description ==
== Description ==
The ParaTech LabTop 3000 Parylene coater uses a multi-stage thermal process to deposit a conformal parylene film on your substrates. Multiple wafers up to 150mm diameter may be coated at once. Samples are under vacuum during and not subject to heat during coating.  
The ParaTech LabTop 3000 Parylene coater uses a multi-stage thermal process to deposit a conformal parylene film on your substrates. Multiple wafers up to 150 mm diameter may be coated at once. Samples are under vacuum during and not subject to heat during coating.


===== Applications =====
===== Applications =====
* Bio-compatible/moisture protection packaging.
* Bio-compatible/moisture protection packaging
* Dielectric polymer coating
* Dielectric polymer coating



Latest revision as of 00:26, 16 July 2025

Parylene Coater
Instrument Type Deposition
Techniques Parylene Deposition
Staff Manager Nathan S. Lee
Staff Email nathslee@caltech.edu
Staff Phone 626-395-4386
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B203 Steele
Lab Phone 626-395-1539
Manufacturer Para Tech
Model LabTop 3000

Description

The ParaTech LabTop 3000 Parylene coater uses a multi-stage thermal process to deposit a conformal parylene film on your substrates. Multiple wafers up to 150 mm diameter may be coated at once. Samples are under vacuum during and not subject to heat during coating.

Applications
  • Bio-compatible/moisture protection packaging
  • Dielectric polymer coating

Resources