Tube Furnaces for Wet & Dry Processing: Difference between revisions
Jump to navigation
Jump to search
m Removed link to Equipment Status under Resources since the status can be viewed directly by users in FBS, per Tiffany 4/15/24 sg |
|||
| (One intermediate revision by one other user not shown) | |||
| Line 22: | Line 22: | ||
* Annealing | * Annealing | ||
===== Allowed Materials ===== | ===== Allowed Materials ===== | ||
* Silicon or sapphire that is completely free of metal or organic contamination | * Silicon, SiNx, or sapphire that is completely free of metal or organic contamination | ||
** Recommended to have undergone a standard RCA clean or similar beforehand | ** Recommended to have undergone a standard RCA clean or similar beforehand | ||
* No other sample material allowed | * No other sample material allowed | ||
* No metal or organic contamination | * No metal or organic contamination | ||
** Wafers must not have been contacted by metal tweezers, etc. without appropriate cleaning to remove metal contamination | ** Wafers must not have been contacted by metal tweezers, etc. without appropriate cleaning to remove metal contamination | ||
===== Gas List ===== | ===== Gas List ===== | ||
* Nitrogen | * Nitrogen | ||
| Line 32: | Line 33: | ||
* Water Vapor (Tube 1) | * Water Vapor (Tube 1) | ||
== Resources == | == Resources == | ||
===== Tystar Oxidation Recipe ===== | ===== Tystar Oxidation Recipe ===== | ||
Latest revision as of 22:59, 15 April 2024
|
Description
The system is designed for processing up to one-hundred, 150 mm (6") silicon or sapphire wafers per tube and can accommodate smaller sample sizes also. Tube 1 is designated for wet & dry oxidation using a flask evaporator. Tube 2 is designated for dry oxidation and annealing.
Applications
- Dry & Wet oxidation
- Annealing
Allowed Materials
- Silicon, SiNx, or sapphire that is completely free of metal or organic contamination
- Recommended to have undergone a standard RCA clean or similar beforehand
- No other sample material allowed
- No metal or organic contamination
- Wafers must not have been contacted by metal tweezers, etc. without appropriate cleaning to remove metal contamination
Gas List
- Nitrogen
- Oxygen
- Water Vapor (Tube 1)