== Description ==
== Description ==
The Solaris 150 is a manual loading Rapid Thermal Processor system that can process up to 6 inch substrates.  The Solaris 150 is designed for silicon implant annealing and monitoring and compound semiconductor implant activation and ohmic alloying.
The Solaris 150 is a manual loading Rapid Thermal Processor system that can process up to 6 inch substrates.  The system is designed for silicon implant annealing and monitoring and compound semiconductor implant activation and ohmic alloying.
===== Applications =====
===== Applications =====
*Temperature range from room temperature to 1200 degrees C.
*Temperature range from room temperature to 1200 degrees C.

Revision as of 21:11, 29 June 2023

Solaris Rapid Thermal Processor
Instrument Type Metrology
Techniques Rapid Thermal Processing
Staff Manager Alireza Ghaffari
Staff Email alireza@caltech.edu
Staff Phone 626-395-3984
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B235 Steele
Lab Phone 626-395-1539
Manufacturer Surface science integration
Model Solaris 150

Description

The Solaris 150 is a manual loading Rapid Thermal Processor system that can process up to 6 inch substrates. The system is designed for silicon implant annealing and monitoring and compound semiconductor implant activation and ohmic alloying.

Applications
  • Temperature range from room temperature to 1200 degrees C.
  • Processing gasses available:
    • Argon
    • Nitrogen
    • Forming Gas

Resources

SOPs
  • SOP coming soon.
Manuals
  • Manual coming soon.