Nova 200 NanoLab: SEM & EDS: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
No edit summary
Line 50: Line 50:
===== Manufacturer Manuals =====
===== Manufacturer Manuals =====
* [https://caltech.box.com/s/og4309108q4k2jwhkaxqtpiujg2al5iu Nova NanoLab Operation Manual]
* [https://caltech.box.com/s/og4309108q4k2jwhkaxqtpiujg2al5iu Nova NanoLab Operation Manual]
* [https://caltech.box.com/s/j0t3w6i53jhfjcva8i4qvlatdh7t1tzw Gas Injection Systems – Deposition of Platinum (Technical Note)]
* [https://caltech.box.com/s/zb5m72tc5c61pegangjjwj3wc8rbj1vr Gas Injection Systems – Deposition of Tungsten (Technical Note)]
* [https://caltech.box.com/s/sm7q7teh5fo5hg3e6flkjbcbycmarrm3 Gas Injection Systems – Deposition of SiOx (Technical Note)]
* [https://caltech.box.com/s/th6cpko7opc9pccn2ukmdc88oh8oa6zw Gas Injection Systems – Delineation Etch for SiO<sub>2</sub>  (Technical Note)]
* [https://caltech.box.com/s/4pcym0l9j1e8t9b2vznrzps9uk7b85mh Gas Injection Systems – Etching with IEE aka XeF2 Etch (Technical Note)]
* [https://caltech.box.com/s/u56ho1hve4pf9713aw09iolukfc8wsb1 Gas Injection Systems – Selective Carbon Etching (Technical Note)]
* [https://caltech.box.com/s/b95pg59k003i9vn8y9elzem0tnxqg3fb Gas Injection Systems – Beam Chemistries Presentation]
* [https://caltech.box.com/s/b95pg59k003i9vn8y9elzem0tnxqg3fb Gas Injection Systems – Beam Chemistries Presentation]
* [https://caltech.box.com/s/110tb0o8avjziwa1y4d017dbbcpkxfop Scripting – AutoScript Language Manual (year 2000 Technical Note: most complete)]
* [https://caltech.box.com/s/110tb0o8avjziwa1y4d017dbbcpkxfop Scripting – AutoScript Language Manual (year 2000 Technical Note: most complete)]
* [https://caltech.box.com/s/n0abqy5z1e9a8hbyf38qybxu86sqz3vb Scripting – AutoScript Language Manual (year 2005 Technical Note: less complete, still useful)]
* [https://caltech.box.com/s/n0abqy5z1e9a8hbyf38qybxu86sqz3vb Scripting – AutoScript Language Manual (year 2005 Technical Note: less complete, still useful)]
* [https://caltech.box.com/s/tlqgvtkkiahi261megm087i61gqlfzrc Scripting – RunScript Manual]
* [https://caltech.box.com/s/tlqgvtkkiahi261megm087i61gqlfzrc Scripting – RunScript Manual]
===== Simulation Software =====
===== Simulation Software =====
* [http://www.gel.usherbrooke.ca/casino/What.html CASINO Electron Beam Simulation Software] – simulate e-beam/specimen interactions
* [http://www.gel.usherbrooke.ca/casino/What.html CASINO Electron Beam Simulation Software] – simulate e-beam/specimen interactions

Revision as of 22:40, 24 April 2019

Nova 200 NanoLab
KNI-Si-and-Pt-Pillar.jpg
Instrument Type Microscopy
Techniques SEM, EDS, WDS,
Immersion Lens Imaging
Staff Manager Matthew S. Hunt, PhD
Staff Email matthew.hunt@caltech.edu
Staff Phone 626-395-5994
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B203 Steele
Lab Phone 626-395-1542
Manufacturer FEI (now Thermo Fisher)
Model {{{Model}}}
Nova-200-NanoLab.jpg

Description

The Nova 200 is the KNI's highest-resolution analytical scanning electron microscope (SEM), equipped with an immersion-lens for imaging sub-10 nm features and both energy dispersive spectroscopy (EDS) and wavelength dispersive spectroscopy (WDS) detectors for compositional analysis. It is also outfitted with a gallium focused ion beam (Ga-FIB) column, which is currently not operational because the Nova 600 NanoLab and ORION NanoFab together meet the KNI's Ga-FIB demand; gallium could be reactivated on the Nova 200 the future. See a full list of training and educational resources for this instrument below.

SEM Applications
  • Ultra-High-Resolution Imaging (Immersion Mode)
  • High-Resolution Imaging (Field-Free Mode)
  • Secondary Electron (SE) & Backscattered Electron (BSE) Imaging
  • Everhart-Thornley Detector (ETD) & Through-the-Lens Detector (TLD)
  • Tungsten deposition via Gas Injection System (GIS)
  • Automated imaging with RunScript program & AutoScript language
Analytical Applications
  • Compositional analysis with EDS (via x-ray detection)
  • Compositional analysis with WDS (via x-ray detection)

Resources

SOPs & Troubleshooting
Video Tutorials
Graphical Handouts
Presentations
Manufacturer Manuals
Simulation Software
Order Your Own Stubs
  • Stubs used for mounting specimens are considered a personal, consumable item in the KNI. There are some old stubs at each SEM, yet you should buy your own so that you can keep them clean and available to you. There are many stub geometries and configurations, some of which will be right for you to purchase and keep with your other cleanroom items.

Specifications

Manufacturer Specifications
Scanning Electron Microscope (SEM) Specifications
  • 0.5 to 30.0 kV
  • Apertures: 10 mm, 15 mm, 20 mmm, 30 mm
  • etc.
Gallium Focused Ion Beam (Ga-FIB) Specifications
  • 5.0 to 30.0 kV
  • 10 pA - 20 nA
  • etc.