Usage Rates: Difference between revisions
No edit summary |
|||
| Line 9: | Line 9: | ||
{| class="wikitable" style="width: 75%;" | {| class="wikitable" style="width: 75%;" | ||
|- | |- | ||
!scope="col" style="text-align:left; width: | !scope="col" style="text-align:left; width: 30%"| Name | ||
!scope="col" style="text-align:center; width: | !scope="col" style="text-align:center; width: 20%"| Category | ||
!scope="col" style="text-align:center; width: | !scope="col" style="text-align:center; width: 15%"| Caltech Rate | ||
!scope="col" style="text-align:center; width: | !scope="col" style="text-align:center; width: 20%"| JPL/Non-Caltech Acad/Govt Rate | ||
!scope="col" style="text-align:center; width: 15%" | Corporate Rate** | |||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = Electron Beam Pattern Generators (100kV) | ||
|EquipmentCategory = Lithography | |||
|CaltechRate = 62.00 | |CaltechRate = 62.00 | ||
|JPLNonCaltechAcadGovtRate = 101.99 | |JPLNonCaltechAcadGovtRate = 101.99 | ||
|CorporateRate = 152.99 | |CorporateRate = 152.99 | ||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = Two-Photon Lithography ("Microscale 3D Printing") | ||
|CaltechRate = | |EquipmentCategory = Lithography | ||
|JPLNonCaltechAcadGovtRate = | |CaltechRate = 8.00 | ||
|CorporateRate = | |JPLNonCaltechAcadGovtRate = 13.16 | ||
|CorporateRate = 19.74 | |||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = Direct-Write Laser System (DWL-66) | ||
|CaltechRate = | |EquipmentCategory = Lithography | ||
|JPLNonCaltechAcadGovtRate = | |CaltechRate = 47.00 | ||
|CorporateRate = | |JPLNonCaltechAcadGovtRate = 77.32 | ||
|CorporateRate = 115.97 | |||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = Contact Mask Aligners | ||
|CaltechRate = | |EquipmentCategory = Lithography | ||
|JPLNonCaltechAcadGovtRate = | |CaltechRate = 36.00 | ||
|CorporateRate = | |JPLNonCaltechAcadGovtRate = 59.22 | ||
|CorporateRate = 88.83 | |||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = He/Ne/Ga-FIB w/ Multibeam Pattern Generator | ||
|EquipmentCategory = Lithography/Microscopy | |||
|CaltechRate = 65.00 | |CaltechRate = 65.00 | ||
|JPLNonCaltechAcadGovtRate = 106.93 | |JPLNonCaltechAcadGovtRate = 106.93 | ||
| Line 44: | Line 51: | ||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = SEM Nanometer Pattern Generation System (Quanta) | ||
|EquipmentCategory = Lithography/Microscopy | |||
|CaltechRate = 39.00 | |CaltechRate = 39.00 | ||
|JPLNonCaltechAcadGovtRate = 64.16 | |JPLNonCaltechAcadGovtRate = 64.16 | ||
| Line 50: | Line 58: | ||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = Etcher: III/V Material, Metal & Silicon | ||
|CaltechRate = | |EquipmentCategory = Etching | ||
|JPLNonCaltechAcadGovtRate = | |CaltechRate = 50.00 | ||
|CorporateRate = | |JPLNonCaltechAcadGovtRate = 82.25 | ||
|CorporateRate = 123.38 | |||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = Etcher: Silicon (DRIE) | ||
|CaltechRate = | |EquipmentCategory = Etching | ||
|JPLNonCaltechAcadGovtRate = | |CaltechRate = 50.00 | ||
|CorporateRate = | |JPLNonCaltechAcadGovtRate = 82.25 | ||
|CorporateRate = 123.38 | |||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = Etcher: Dielectric Material ("380") | ||
|EquipmentCategory = Etching | |||
|CaltechRate = 50.00 | |CaltechRate = 50.00 | ||
|JPLNonCaltechAcadGovtRate = 82.25 | |JPLNonCaltechAcadGovtRate = 82.25 | ||
| Line 68: | Line 79: | ||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = Etcher: Silicon, III/V Material & Organics (RIE) | ||
|EquipmentCategory = Etching | |||
|CaltechRate = 50.00 | |CaltechRate = 50.00 | ||
|JPLNonCaltechAcadGovtRate = 82.25 | |JPLNonCaltechAcadGovtRate = 82.25 | ||
| Line 74: | Line 86: | ||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = XeF<sub>2</sub> Etcher | ||
|EquipmentCategory = Etching | |||
|CaltechRate = 50.00 | |CaltechRate = 50.00 | ||
|JPLNonCaltechAcadGovtRate = 82.25 | |JPLNonCaltechAcadGovtRate = 82.25 | ||
| Line 80: | Line 93: | ||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = Plasma-Enhanced Chemical Vapor Deposition | ||
|EquipmentCategory = Deposition | |||
|CaltechRate = 67.00 | |CaltechRate = 67.00 | ||
|JPLNonCaltechAcadGovtRate = 110.22 | |JPLNonCaltechAcadGovtRate = 110.22 | ||
| Line 86: | Line 100: | ||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = Atomic Layer Deposition | ||
|EquipmentCategory = Deposition | |||
|CaltechRate = 67.00 | |CaltechRate = 67.00 | ||
|JPLNonCaltechAcadGovtRate = 110.22 | |JPLNonCaltechAcadGovtRate = 110.22 | ||
| Line 92: | Line 107: | ||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = E-beam Evaporator: Metals and Oxides (CHA) | ||
|EquipmentCategory = Deposition | |||
|CaltechRate = 24.00 | |CaltechRate = 24.00 | ||
|JPLNonCaltechAcadGovtRate = 39.48 | |JPLNonCaltechAcadGovtRate = 39.48 | ||
| Line 110: | Line 114: | ||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = E-beam Evaporator: Metals Al, Au, Pt & Ti (Lesker Labline) | ||
|EquipmentCategory = Deposition | |||
|CaltechRate = 24.00 | |CaltechRate = 24.00 | ||
|JPLNonCaltechAcadGovtRate = 39.48 | |JPLNonCaltechAcadGovtRate = 39.48 | ||
| Line 117: | Line 122: | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = Chalcogenide Sputter | |EquipmentName = Chalcogenide Sputter | ||
|EquipmentCategory = Deposition | |||
|CaltechRate = 70.00 | |CaltechRate = 70.00 | ||
|JPLNonCaltechAcadGovtRate = 115.15 | |JPLNonCaltechAcadGovtRate = 115.15 | ||
| Line 123: | Line 129: | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = Dielectric Sputter | |EquipmentName = Dielectric Sputter | ||
|EquipmentCategory = Deposition | |||
|CaltechRate = 37.00 | |CaltechRate = 37.00 | ||
|JPLNonCaltechAcadGovtRate = 60.87 | |JPLNonCaltechAcadGovtRate = 60.87 | ||
| Line 128: | Line 135: | ||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = SEM, EDS & WDS (Nova 200) | ||
|CaltechRate = | |EquipmentCategory = Microscopy | ||
|JPLNonCaltechAcadGovtRate = | |CaltechRate = 65.00 | ||
|CorporateRate = | |JPLNonCaltechAcadGovtRate = 106.93 | ||
|CorporateRate = 160.39 | |||
}} | |||
{{UsageRateTableItem| | |||
|EquipmentName = SEM, Ga-FIB, GIS & Omniprobe (Nova 600) | |||
|EquipmentCategory = Microscopy | |||
|CaltechRate = 65.00 | |||
|JPLNonCaltechAcadGovtRate = 106.93 | |||
|CorporateRate = 160.39 | |||
}} | |||
{{UsageRateTableItem| | |||
|EquipmentName = SEM & EDS (Sirion) | |||
|EquipmentCategory = Microscopy | |||
|CaltechRate = 39.00 | |||
|JPLNonCaltechAcadGovtRate = 64.16 | |||
|CorporateRate = 96.23 | |||
}} | |||
{{UsageRateTableItem| | |||
|EquipmentName = Atomic Force Microscope | |||
|EquipmentCategory = Microscopy | |||
|CaltechRate = 41.00 | |||
|JPLNonCaltechAcadGovtRate = 67.45 | |||
|CorporateRate = 101.17 | |||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = TEM, STEM, EDS & HAADF: TF-30 (80-300 kV) | ||
|CaltechRate = | |EquipmentCategory = Microscopy | ||
|JPLNonCaltechAcadGovtRate = | |CaltechRate = 97.00 | ||
|CorporateRate = | |JPLNonCaltechAcadGovtRate = 159.57 | ||
|CorporateRate = 239.35 | |||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = | |EquipmentName = Critical Point Dryer | ||
|EquipmentCategory = Support Tools | |||
|CaltechRate = 54.00 | |CaltechRate = 54.00 | ||
|JPLNonCaltechAcadGovtRate = 88.83 | |JPLNonCaltechAcadGovtRate = 88.83 | ||
|CorporateRate = 133.25 | |CorporateRate = 133.25 | ||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = Tube Furnaces | |EquipmentName = Tube Furnaces | ||
|EquipmentCategory = Support Tools | |||
|CaltechRate = 5.00 | |CaltechRate = 5.00 | ||
|JPLNonCaltechAcadGovtRate = 8.23 | |JPLNonCaltechAcadGovtRate = 8.23 | ||
|CorporateRate = 12.34 | |CorporateRate = 12.34 | ||
}} | }} | ||
{{UsageRateTableItem| | {{UsageRateTableItem| | ||
|EquipmentName = Monthly Base Rate* | |EquipmentName = Monthly Base Rate* | ||
|EquipmentCategory = General Equipment* | |||
|CaltechRate = 655.00 | |CaltechRate = 655.00 | ||
|JPLNonCaltechAcadGovtRate = 1,077.48 | |JPLNonCaltechAcadGovtRate = 1,077.48 | ||
| Line 174: | Line 195: | ||
The Monthly Base Rate is a flat fee charged per user, per month. It includes the use of: | The Monthly Base Rate is a flat fee charged per user, per month. It includes the use of: | ||
Profilometers, Chemical Wet Benches, Dynatex GST-150 Scriber Breaker, | Profilometers, Chemical Wet Benches, Dynatex GST-150 Scriber Breaker, J.A. Woolam Spectroscopic Ellipsometer M-2000, TF20 TEM, GCA 6300 Stepper, Rapid Thermal Processor, Paratech Parylene Coater, Suss SB6L Wafer Bonder, Westbond Wire Bonder, additional optical microscopes, related metrology, miscellaneous support tools and general supplies (gowning, chemicals, equipment reservation software, etc.). | ||
==**Corporate Memberships== | ==**Corporate Memberships== | ||
For full information on the KNI's corporate membership plan, please send an email to tkimoto@caltech.edu with details regarding: the number of people looking to join as KNI lab members, equipment needs, anticipated start date, and information about the company. Startup companies may qualify for limited-term reduced rates. | For full information on the KNI's corporate membership plan, please send an email to tkimoto@caltech.edu with details regarding: the number of people looking to join as KNI lab members, equipment needs, anticipated start date, and information about the company. Startup companies may qualify for limited-term reduced rates. | ||
Revision as of 02:15, 30 April 2019
The rates below are valid beginning October 2018 and are subject to change.
NOTE:
- Rates for JPL, Non-Caltech Academic, Government, and Corporate KNI lab members are inclusive of FY19 Caltech F&A ("overhead") fees.
- Individual Tools listed below are charged by the hour or portion thereof.
- Precious Metal Usage (e.g. gold, platinum) is billed by the gram or portion thereof. The market prices per gram are passed on to users and do not include Caltech overhead.
Equipment Rates
| Name | Category | Caltech Rate | JPL/Non-Caltech Acad/Govt Rate | Corporate Rate** |
|---|---|---|---|---|
| Electron Beam Pattern Generators (100kV) |
Lithography |
$62.00 |
$101.99 |
$152.99 |
| Two-Photon Lithography ("Microscale 3D Printing") |
Lithography |
$8.00 |
$13.16 |
$19.74 |
| Direct-Write Laser System (DWL-66) |
Lithography |
$47.00 |
$77.32 |
$115.97 |
| Contact Mask Aligners |
Lithography |
$36.00 |
$59.22 |
$88.83 |
| He/Ne/Ga-FIB w/ Multibeam Pattern Generator |
Lithography/Microscopy |
$65.00 |
$106.93 |
$160.39 |
| SEM Nanometer Pattern Generation System (Quanta) |
Lithography/Microscopy |
$39.00 |
$64.16 |
$96.23 |
| Etcher: III/V Material, Metal & Silicon |
Etching |
$50.00 |
$82.25 |
$123.38 |
| Etcher: Silicon (DRIE) |
Etching |
$50.00 |
$82.25 |
$123.38 |
| Etcher: Dielectric Material ("380") |
Etching |
$50.00 |
$82.25 |
$123.38 |
| Etcher: Silicon, III/V Material & Organics (RIE) |
Etching |
$50.00 |
$82.25 |
$123.38 |
| XeF2 Etcher |
Etching |
$50.00 |
$82.25 |
$123.38 |
| Plasma-Enhanced Chemical Vapor Deposition |
Deposition |
$67.00 |
$110.22 |
$165.32 |
| Atomic Layer Deposition |
Deposition |
$67.00 |
$110.22 |
$165.32 |
| E-beam Evaporator: Metals and Oxides (CHA) |
Deposition |
$24.00 |
$39.48 |
$59.22 |
| E-beam Evaporator: Metals Al, Au, Pt & Ti (Lesker Labline) |
Deposition |
$24.00 |
$39.48 |
$59.22 |
| Chalcogenide Sputter |
Deposition |
$70.00 |
$115.15 |
$172.73 |
| Dielectric Sputter |
Deposition |
$37.00 |
$60.87 |
$91.30 |
| SEM, EDS & WDS (Nova 200) |
Microscopy |
$65.00 |
$106.93 |
$160.39 |
| SEM, Ga-FIB, GIS & Omniprobe (Nova 600) |
Microscopy |
$65.00 |
$106.93 |
$160.39 |
| SEM & EDS (Sirion) |
Microscopy |
$39.00 |
$64.16 |
$96.23 |
| Atomic Force Microscope |
Microscopy |
$41.00 |
$67.45 |
$101.17 |
| TEM, STEM, EDS & HAADF: TF-30 (80-300 kV) |
Microscopy |
$97.00 |
$159.57 |
$239.35 |
| Critical Point Dryer |
Support Tools |
$54.00 |
$88.83 |
$133.25 |
| Tube Furnaces |
Support Tools |
$5.00 |
$8.23 |
$12.34 |
| Monthly Base Rate* |
General Equipment* |
$655.00 |
$1,077.48 |
$1,616.21 |
*Monthly Base Rate
The Monthly Base Rate is a flat fee charged per user, per month. It includes the use of:
Profilometers, Chemical Wet Benches, Dynatex GST-150 Scriber Breaker, J.A. Woolam Spectroscopic Ellipsometer M-2000, TF20 TEM, GCA 6300 Stepper, Rapid Thermal Processor, Paratech Parylene Coater, Suss SB6L Wafer Bonder, Westbond Wire Bonder, additional optical microscopes, related metrology, miscellaneous support tools and general supplies (gowning, chemicals, equipment reservation software, etc.).
**Corporate Memberships
For full information on the KNI's corporate membership plan, please send an email to tkimoto@caltech.edu with details regarding: the number of people looking to join as KNI lab members, equipment needs, anticipated start date, and information about the company. Startup companies may qualify for limited-term reduced rates.