Process Recipe Library: Difference between revisions
		
		
		
		Jump to navigation
		Jump to search
		
| Line 44: | Line 44: | ||
| ===== Scanning Electron Microscopes (SEMs) ===== | ===== Scanning Electron Microscopes (SEMs) ===== | ||
| * [https://caltech.box.com/s/e5cdnag69i2w9nm1d0p07fyun4k15b5c Environmental SEM (ESEM) Imaging Guide (for biological and highly non-conductive specimens)] | * [https://caltech.box.com/s/e5cdnag69i2w9nm1d0p07fyun4k15b5c Environmental SEM (ESEM) Imaging Guide (for biological and highly non-conductive specimens)] | ||
| * [https://caltech.box.com/s/vg9rpa4ac9e1eki79hfecccpohl3qp6u Performing Aligned EBL Patterning Steps with NPGS on an SEM] | [https://caltech.box.com/s/tl4bliegxptu5tfmzu0p7vs1hcnxtyj8 Alignment Template Files] | |||
| ===== Transmission Electron Microscopes (TEMs) ===== | ===== Transmission Electron Microscopes (TEMs) ===== | ||
| * [https://caltech.box.com/s/fwhkep9qf3bhdygshvfi4dycy2qpmi0i STEM mode EDS on TF-20 TEM (emphasis on high-resolution 2D mapping)] | * [https://caltech.box.com/s/fwhkep9qf3bhdygshvfi4dycy2qpmi0i STEM mode EDS on TF-20 TEM (emphasis on high-resolution 2D mapping)] | ||
Revision as of 07:54, 30 January 2020
You can browse the available recipes below, by lab area. You can also browse directly within the KNI's Box directory. Note that the vast majority of recipes are being made publicly available; only a select few are password-protected for members of the Caltech community:
- All Content (requires login with a caltech.edu email address)
- Publicly available content (no login required)
Lithography Process Recipes
Electron Beam Lithography
- ZEP 520A Resist: Procedure for spinning, writing & development (Caltech-only access)
- HSQ Resist: Procedure for spinning, writing & development (Caltech-only access)
- Performing Aligned EBL Patterning Steps with NPGS on an SEM | Alignment Template Files
Helium Ion Beam Lithography
Optical Lithography
Deposition Process Recipes
Sputtering
- TiO2 sputtering ecipe
- Aluminum Nitride sputtering recipe
- Al2O3 sputtering recipe
- Guide to maintaining a plasma using gradual pressure changes
Chemical Vapor Deposition (CVD)
Etching Process Recipes
Dry Etching
Wet Etching
Microscopy Process Recipes
Focused Ion Beam (FIB) Systems
- Cutting & Imaging Cross-sections with SEM/Ga-FIB
- Preparing TEM Lamella Samples with SEM/Ga-FIB
- Helium Ion Beam Lithography (HIBL) – Parameter Guide
- Helium Ion Beam Imaging with the Electron Flood Gun – Parameter Guide
- Source Rebuild Guide for ORION NanoFab He- & Ne-FIB
Scanning Electron Microscopes (SEMs)
- Environmental SEM (ESEM) Imaging Guide (for biological and highly non-conductive specimens)
- Performing Aligned EBL Patterning Steps with NPGS on an SEM | Alignment Template Files