Process Recipe Library: Difference between revisions
Jump to navigation
Jump to search
| Line 35: | Line 35: | ||
* [https://caltech.box.com/s/1nmp75l3166vj9t1vwwpwu2zyfc4j6ol Cutting & Imaging Cross-sections with SEM/Ga-FIB] | * [https://caltech.box.com/s/1nmp75l3166vj9t1vwwpwu2zyfc4j6ol Cutting & Imaging Cross-sections with SEM/Ga-FIB] | ||
* [https://caltech.box.com/s/3l3w507dxwosuya3nbxgk30tdqyp4qy9 Preparing TEM Lamella Samples with SEM/Ga-FIB] | * [https://caltech.box.com/s/3l3w507dxwosuya3nbxgk30tdqyp4qy9 Preparing TEM Lamella Samples with SEM/Ga-FIB] | ||
* [https://caltech.box.com/s/3s0k77mgx26ytfnafttpoalcknmk7npu Helium Ion Beam Lithography (HIBL) – Parameter | * [https://caltech.box.com/s/3s0k77mgx26ytfnafttpoalcknmk7npu Helium Ion Beam Lithography (HIBL) – Parameter Guide] | ||
* [https://caltech.box.com/s/qobquoi3hs0izeyhdg5d8px9wmmdzuxw Source | * [https://caltech.box.com/s/ybdwd4zi39p62bx13rc7f8o54444vuyz Helium Ion Beam Imaging with the Electron Flood Gun – Parameter Guide] | ||
* [https://caltech.box.com/s/qobquoi3hs0izeyhdg5d8px9wmmdzuxw Source Rebuild Guide for ORION NanoFab He- & Ne-FIB] | |||
===== Scanning Electron Microscopes (SEMs) ===== | ===== Scanning Electron Microscopes (SEMs) ===== | ||
Revision as of 03:57, 5 December 2019
You can browse the available recipes below, by lab area. You can also browse directly within the KNI's Box directory. Note that the vast majority of recipes are being made publicly available; only a select few are password-protected for members of the Caltech community:
- All Content (requires login with a caltech.edu email address)
- Publicly available content (no login required)
Lithography Process Recipes
Electron Beam Lithography
Helium Ion Beam Lithography
Optical Lithography
Deposition Process Recipes
Sputtering
- TiO2 sputtering ecipe
- Guide to maintaining a plasma using gradual pressure changes
- AlN sputtering recipe
- Al2O3 sputtering recipe
Chemical Vapor Deposition (CVD)
Etching Process Recipes
Dry Etching
Wet Etching
Microscopy Process Recipes
Focused Ion Beam (FIB) Systems
- Cutting & Imaging Cross-sections with SEM/Ga-FIB
- Preparing TEM Lamella Samples with SEM/Ga-FIB
- Helium Ion Beam Lithography (HIBL) – Parameter Guide
- Helium Ion Beam Imaging with the Electron Flood Gun – Parameter Guide
- Source Rebuild Guide for ORION NanoFab He- & Ne-FIB