Process Recipe Library: Difference between revisions
Jump to navigation
Jump to search
| Line 29: | Line 29: | ||
* [https://caltech.box.com/s/1nmp75l3166vj9t1vwwpwu2zyfc4j6ol Cutting & Imaging Cross-sections with SEM/Ga-FIB] | * [https://caltech.box.com/s/1nmp75l3166vj9t1vwwpwu2zyfc4j6ol Cutting & Imaging Cross-sections with SEM/Ga-FIB] | ||
* [https://caltech.box.com/s/3l3w507dxwosuya3nbxgk30tdqyp4qy9 Preparing TEM Lamella Samples with SEM/Ga-FIB] | * [https://caltech.box.com/s/3l3w507dxwosuya3nbxgk30tdqyp4qy9 Preparing TEM Lamella Samples with SEM/Ga-FIB] | ||
* [https://caltech.box.com/s/3s0k77mgx26ytfnafttpoalcknmk7npu Helium Ion Beam Lithography (HIBL) – Parameter Recipe] | |||
* [https://caltech.box.com/s/qobquoi3hs0izeyhdg5d8px9wmmdzuxw Source rebuild guide for ORION NanoFab He- & Ne-FIB] | * [https://caltech.box.com/s/qobquoi3hs0izeyhdg5d8px9wmmdzuxw Source rebuild guide for ORION NanoFab He- & Ne-FIB] | ||
===== Scanning Electron Microscopes (SEMs) ===== | ===== Scanning Electron Microscopes (SEMs) ===== | ||
* [https://caltech.box.com/s/e5cdnag69i2w9nm1d0p07fyun4k15b5c Environmental SEM (ESEM) Imaging Guide (for biological and highly non-conductive specimens)] | * [https://caltech.box.com/s/e5cdnag69i2w9nm1d0p07fyun4k15b5c Environmental SEM (ESEM) Imaging Guide (for biological and highly non-conductive specimens)] | ||
===== Transmission Electron Microscopes (TEMs) ===== | ===== Transmission Electron Microscopes (TEMs) ===== | ||
* [https://caltech.box.com/s/fwhkep9qf3bhdygshvfi4dycy2qpmi0i STEM mode EDS on TF-20 TEM (emphasis on high-resolution 2D mapping)] | * [https://caltech.box.com/s/fwhkep9qf3bhdygshvfi4dycy2qpmi0i STEM mode EDS on TF-20 TEM (emphasis on high-resolution 2D mapping)] | ||
Revision as of 16:16, 27 November 2019
You can browse the available recipes below, by lab area. You can also browse directly within the KNI's Box directory. Note that the vast majority of recipes are being made publicly available; only a select few are password-protected for members of the Caltech community:
- All Content (requires login with a caltech.edu email address)
- Publicly available content (no login required)
Lithography Process Recipes
Electron Beam Lithography
Helium Ion Beam Lithography
Optical Lithography
Deposition Process Recipes
Sputtering
Chemical Vapor Deposition (CVD)
Etching Process Recipes
Dry Etching
Microscopy Process Recipes
Focused Ion Beam (FIB) Systems
- Cutting & Imaging Cross-sections with SEM/Ga-FIB
- Preparing TEM Lamella Samples with SEM/Ga-FIB
- Helium Ion Beam Lithography (HIBL) – Parameter Recipe
- Source rebuild guide for ORION NanoFab He- & Ne-FIB