===== Optical Lithography ===== | ===== Optical Lithography ===== | ||
* [https://caltech.box.com/s/5ls5rk4oanod66pfilsuendthutcmfqu AZ5214 Photoresist spinning procedure] | * [https://caltech.box.com/s/5ls5rk4oanod66pfilsuendthutcmfqu AZ5214 Photoresist spinning procedure] | ||
* [https://caltech.box.com/s/xqwbmcj7l4itj6nqp6lbo7h4vexee0tr AZ9260 Photoresist spinning procedure] | |||
* [https://caltech.box.com/s/6et86m5wlrjf80ew9yo0v8rgjifsdzfs AZ nLof 2000 Photoresist Recipe] | |||
* [https://caltech.box.com/s/3pa2im5jj1e86rdozwigt8yfnb8fi5k3 S1813 Photoresist spinning procedure] | * [https://caltech.box.com/s/3pa2im5jj1e86rdozwigt8yfnb8fi5k3 S1813 Photoresist spinning procedure] | ||
== Deposition Process Recipes == | == Deposition Process Recipes == | ||
Revision as of 14:34, 7 February 2020
You can browse the available recipes below, by lab area. You can also browse directly within the KNI's Box directory. Note that the vast majority of recipes are being made publicly available; only a select few are password-protected for members of the Caltech community:
- All Content (requires login with a caltech.edu email address)
- Publicly available content (no login required)
Lithography Process Recipes
Electron Beam Lithography
- KNI Introduction to BEAMER
- How to Spin Photoresist onto Wafers and Pieces (Video)
- ZEP 520A Resist: Procedure for spinning, writing & development (Caltech-only access)
- HSQ Resist: Procedure for spinning, writing & development (Caltech-only access)
- Performing Aligned EBL Patterning Steps with NPGS on an SEM | Alignment Template Files
Helium Ion Beam Lithography
Optical Lithography
- AZ5214 Photoresist spinning procedure
- AZ9260 Photoresist spinning procedure
- AZ nLof 2000 Photoresist Recipe
- S1813 Photoresist spinning procedure
Deposition Process Recipes
Sputtering
- SnO2 sputtering recipe
- NbOx sputtering recipe
- TiO2 sputtering recipe
- AlN sputtering recipe
- Al2O3 sputtering recipe
- Guide to maintaining a plasma using gradual pressure changes
Chemical Vapor Deposition (CVD)
Etching Process Recipes
Dry Etching
- Comparison of etch rates using different sample-fixing oils
- In-situ (dielectric sputter) RF plasma etch of thermal SiO2
Wet Etching
Microscopy Process Recipes
Focused Ion Beam (FIB) Systems
- Cutting & Imaging Cross-sections with SEM/Ga-FIB
- Preparing TEM Lamella Samples with SEM/Ga-FIB
- Helium Ion Beam Lithography (HIBL) – Parameter Guide
- Helium Ion Beam Imaging with the Electron Flood Gun – Parameter Guide
- Source Rebuild Guide for ORION NanoFab He- & Ne-FIB
Scanning Electron Microscopes (SEMs)
- Environmental SEM (ESEM) Imaging Guide (for biological and highly non-conductive specimens)
- Performing Aligned EBL Patterning Steps with NPGS on an SEM | Alignment Template Files