== Deposition Process Recipes ==
== Deposition Process Recipes ==
===== Sputtering =====
===== Sputtering =====
* [https://caltech.box.com/s/95qrpvvggcaztmpc7whd9v9o4d9rih5x TiO<sub>2</sub> sputtering ecipe]
* [https://caltech.box.com/s/z043k1ne91oowp70lzt69kau0u2nq79f SnO<sub>2</sub> sputtering recipe]
* [https://caltech.box.com/s/oxxv5sy3j7wbqyjc8r9x2wqheabne2lg NbO<sub>x</sub> sputtering recipe]
* [https://caltech.box.com/s/95qrpvvggcaztmpc7whd9v9o4d9rih5x TiO<sub>2</sub> sputtering recipe]
* [https://caltech.box.com/s/k669kh04xglamkidhuo7xq04xan146xt Aluminum Nitride sputtering recipe]
* [https://caltech.box.com/s/k669kh04xglamkidhuo7xq04xan146xt Aluminum Nitride sputtering recipe]
* [https://caltech.box.com/s/7cqdk2g5ic2wa35lu4y2fu03esfk7sdy Al<sub>2</sub>O<sub>3</sub> sputtering recipe]
* [https://caltech.box.com/s/7cqdk2g5ic2wa35lu4y2fu03esfk7sdy Al<sub>2</sub>O<sub>3</sub> sputtering recipe]

Revision as of 19:15, 4 February 2020

You can browse the available recipes below, by lab area. You can also browse directly within the KNI's Box directory. Note that the vast majority of recipes are being made publicly available; only a select few are password-protected for members of the Caltech community:

  1. All Content (requires login with a caltech.edu email address)
  2. Publicly available content (no login required)


Lithography Process Recipes

Electron Beam Lithography
Helium Ion Beam Lithography
Optical Lithography

Deposition Process Recipes

Sputtering
Chemical Vapor Deposition (CVD)

Etching Process Recipes

Dry Etching
Wet Etching

Microscopy Process Recipes

Focused Ion Beam (FIB) Systems
Scanning Electron Microscopes (SEMs)
Transmission Electron Microscopes (TEMs)