Process Recipe Library: Difference between revisions
Jump to navigation
Jump to search
Created page with "You can browse the available recipes below, by lab area. You can also browse directly within the KNI's Process Recipe Libraries: # [https://caltech.app.box.com/folder/89929833..." |
mNo edit summary |
||
| Line 1: | Line 1: | ||
You can browse the available recipes below, by lab area. You can also browse directly within the KNI's | You can browse the available recipes below, by lab area. You can also browse directly within the KNI's folder directories: | ||
# [https://caltech.app.box.com/folder/89929833301 All Content (requires login with a caltech.edu email address)] | # [https://caltech.app.box.com/folder/89929833301 All Content (requires login with a caltech.edu email address)] | ||
# [https://caltech.box.com/s/uqtkc7xev3xvda2ueykt7cj1886ok1mg Publicly available content (no login required)] | # [https://caltech.box.com/s/uqtkc7xev3xvda2ueykt7cj1886ok1mg Publicly available content (no login required)] | ||
== Lithography Process Recipes == | == Lithography Process Recipes == | ||
===== Electron Beam Lithography ===== | ===== Electron Beam Lithography ===== | ||
* [https://caltech.box.com/s/m1vf71b2df8zffiz7hp4p1ay6p6kv4k9 ZEP 520A resist spinning procedure ( | * [https://caltech.box.com/s/m1vf71b2df8zffiz7hp4p1ay6p6kv4k9 ZEP 520A resist spinning procedure (Caltech-only access)] | ||
===== Optical Lithography ===== | ===== Optical Lithography ===== | ||
* [https://caltech.box.com/s/5ls5rk4oanod66pfilsuendthutcmfqu AZ5214 resist spinning recipe] | * [https://caltech.box.com/s/5ls5rk4oanod66pfilsuendthutcmfqu AZ5214 resist spinning recipe] | ||
Revision as of 23:53, 7 November 2019
You can browse the available recipes below, by lab area. You can also browse directly within the KNI's folder directories:
- All Content (requires login with a caltech.edu email address)
- Publicly available content (no login required)