Wet Chemistry Resources: Difference between revisions
Jump to navigation
Jump to search
Line 12: | Line 12: | ||
==Solvent Cleans== | ==Solvent Cleans== | ||
*[https://www-s.mechse.uiuc.edu/cleanroom/files/Procedures/Process/Wafer%20Cleaning%20Procedure%20V1.0.pdf UIUC Wafer Cleaning Procedure] | |||
*'''Acetone, IPA''' -Acetone serves as a solvent for organics, IPA cleans remaining residues due to acetone's high evaporation rate | *'''Acetone, IPA''' -Acetone serves as a solvent for organics, IPA cleans remaining residues due to acetone's high evaporation rate |
Revision as of 11:50, 1 November 2019
Sample Cleaning Resources
Solvent Cleans
- Acetone, IPA -Acetone serves as a solvent for organics, IPA cleans remaining residues due to acetone's high evaporation rate
- Acetone, Methanol -Similar to above except Methanol is more toxic, and a polar chemical versus IPA which is non-polar
- Acetone, Methanol, IPA
- Acetone, Methanol, IPA, DI Water
- Remover PG (50°C), IPA
- Dichloromethane, IPA -Caution, high evaporation rate may leave residue and beakers quickly condense water/ice
- Nanostrip (60°C) -rinse with DI
Etching Cleans
RCA-1
Recipe steps or links
https://en.wikipedia.org/wiki/RCA_clean
Piranha Etch
HF Dip
Plasma Cleans
Wet Etching Resources
find etch list book and other links
Research Papers and Books
External Laboratories
also find alternative:
Commercial Materials
KNI Wet Etch Recipes Table
Table of Wet Etch recipes from KNI Papers
And general table from you, not from papers, maybe from recipes?
Material | Etchant | Rate (nm/min) | Anisotropy | Selective to | Selectivity | Origin and Notes |
---|---|---|---|---|---|---|
KNI CHA Al | Al Etch Type D | ~1000 | Highly | Al | High | Matches Transene's expected rate |
KNI PECVD SiO2 | HF | ~1000 | Highly | SiO2 | High | measured 10/19 |
KNI PECVD SiN3 | Ex | ~1000 | Highly | SiN3 | High | measured 10/19 |
KNI PECVD a-Si | KOH | ~1000 | Highly | Si | High | Link to KNI member's research paper |
Other Procedures
Liftoff
Electroplating
Safety Resources
Do we have materials to link to?
https://cleanroom.byu.edu/acid_safety