Process Recipe Library: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
mNo edit summary
Line 8: Line 8:
* [https://caltech.app.box.com/file/549582924881 ZEP 520A resist spinning procedure (Caltech-only access)]
* [https://caltech.app.box.com/file/549582924881 ZEP 520A resist spinning procedure (Caltech-only access)]
===== Optical Lithography =====
===== Optical Lithography =====
* [https://caltech.box.com/s/5ls5rk4oanod66pfilsuendthutcmfqu AZ5214 resist spinning recipe]
* [https://caltech.box.com/s/5ls5rk4oanod66pfilsuendthutcmfqu AZ5214 resist spinning procedure]
* [https://caltech.box.com/s/quqnspqndxtyo8jz0l37j7n9n3l40w5a S1813 resist spinning recipe]
* [https://caltech.box.com/s/quqnspqndxtyo8jz0l37j7n9n3l40w5a S1813 resist spinning procedure]


== Deposition Process Recipes ==
== Deposition Process Recipes ==

Revision as of 02:51, 8 November 2019

You can browse the available recipes below, by lab area. You can also browse directly within the KNI's Box directory. Note that the vast majority of recipes are being made publicly available; only a select few are password-protected for members of the Caltech community:

  1. All Content (requires login with a caltech.edu email address)
  2. Publicly available content (no login required)


Lithography Process Recipes

Electron Beam Lithography
Optical Lithography

Deposition Process Recipes

Sputtering
Chemical Vapor Deposition (CVD)

Etching Process Recipes

Dry Etching

Microscopy Process Recipes

Focused Ion Beam (FIB) Systems
Scanning Electron Microscopes (SEMs)
Transmission Electron Microscopes (TEMs)