* [https://caltech.app.box.com/file/549582924881 ZEP 520A Resist: Procedure for spinning, writing & development (Caltech-only access)]
* [https://caltech.app.box.com/file/549582924881 ZEP 520A Resist: Procedure for spinning, writing & development (Caltech-only access)]
* [https://caltech.box.com/s/lijnz00qwpk7z5qbz8kn9tjo0kqfgz4a HSQ Resist: Procedure for spinning, writing & development (Caltech-only access)]
* [https://caltech.box.com/s/lijnz00qwpk7z5qbz8kn9tjo0kqfgz4a HSQ Resist: Procedure for spinning, writing & development (Caltech-only access)]
* [https://caltech.box.com/s/vg9rpa4ac9e1eki79hfecccpohl3qp6u Performing Aligned EBL Patterning Steps with NPGS on an SEM] | [https://caltech.box.com/s/tl4bliegxptu5tfmzu0p7vs1hcnxtyj8 Alignment Template Files]


===== Helium Ion Beam Lithography =====
===== Helium Ion Beam Lithography =====

Revision as of 07:53, 30 January 2020

You can browse the available recipes below, by lab area. You can also browse directly within the KNI's Box directory. Note that the vast majority of recipes are being made publicly available; only a select few are password-protected for members of the Caltech community:

  1. All Content (requires login with a caltech.edu email address)
  2. Publicly available content (no login required)


Lithography Process Recipes

Electron Beam Lithography
Helium Ion Beam Lithography
Optical Lithography

Deposition Process Recipes

Sputtering
Chemical Vapor Deposition (CVD)

Etching Process Recipes

Dry Etching
Wet Etching

Microscopy Process Recipes

Focused Ion Beam (FIB) Systems
Scanning Electron Microscopes (SEMs)
Transmission Electron Microscopes (TEMs)